Creep Failure Analysis of Steel Tubes
-
Published:2019
Abstract
Failures of 10Cr-Mo9-10 and X 20Cr-Mo-V12-1 superheated pipes during service in steam power generation plants are described. Through micrographic and fractographic analysis, creep and overheating were identified as the cause of failure. The Larson-Miller parameter is computed, as a function of oxidation thickness, temperature and time, confirming the creep failure diagnostic.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
J.A. Pero-Sanz, D. Plaza, M. Ruiz, J. Asensio, J.I. Verdeja, Creep Failure Analysis of Steel Tubes, ASM Failure Analysis Case Histories: Power Generating Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.power.c9001711
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Combined EDX/AES Analysis of Failed Inconel 600 Steam Line Bellows
ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment
Stress-Corrosion Cracking Failure of a Sensitized Valve Stem
ASM Failure Analysis Case Histories: Power Generating Equipment
Failure of a Steel Superheater Tube
ASM Failure Analysis Case Histories: Power Generating Equipment
Failure Investigation of Longitudinal Seam Welded Elevated Temperature Header
ASM Failure Analysis Case Histories: Power Generating Equipment
Failure of a Main Steam Line of a Power-Generating Station
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Rivet-Hole Cracks in a Steam Boiler
ASM Failure Analysis Case Histories: Rail and Rolling Stock
Failure of a Boiler Feed Pump Second-Stage Impeller
Handbook of Case Histories in Failure Analysis
Creep Failure of a 2.25Cr-1Mo Steel Superheater Tube
ASM Failure Analysis Case Histories: Improper Maintenance, Repair, and Operating Conditions
Failure Analysis of Boiler Water Wall-Tubes at a Power Generation Plant
ASM Failure Analysis Case Histories: Power Generating Equipment
Fracture of Steam Pipes Removed From Service
Handbook of Case Histories in Failure Analysis