Another Turbogenerator Failure
By
R. James Landrum
R. James Landrum
Group Supervisor, Applied Engineering Materials, Engineering Service Div., Engineering Dept., E. I. du Pont de Nemours & Co.
Search for other works by this author on:
-
Published:2019
Abstract
Another failure in a turbogenerator, similar to the accidents in Toronto described in Metal Progress in July 1956, was due to the presence of fatigue cracks at ventilating holes. These acted as stress-raisers during temporary and minor overspeeding, inducing an almost instantaneous brittle failure which wrecked the machine, fortunately without human casualty.
You do not currently have access to this chapter.
Citation
R. James Landrum, Another Turbogenerator Failure, ASM Failure Analysis Case Histories: Power Generating Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.power.c9001725
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Failures of Forged End Bells on Large Electric Generators
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Brittle Fracture of a Cadmium-Plated 4140 Steel Retaining Ring at a Hard Spot Caused by an Arc Strike
ASM Failure Analysis Case Histories: Mechanical and Machine Components
Brittle Fracture of a Roll-Assembly Sleeve Due to Improper Microstructure
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Brittle Fracture of Rocket-Motor Case That Originated at Delayed Quench Cracks
ASM Failure Analysis Case Histories: Processing Errors and Defects
Failure of a Structural Bolt Due to Reversed-Bending Fatigue
ASM Failure Analysis Case Histories: Buildings, Bridges, and Infrastructure
Redesign of a Forged Manual Gear-Shift Lever Mechanism to Overcome Unacceptable Fatigue Failure of Original Forging
ASM Failure Analysis Case Histories: Automobiles and Trucks
Fatigue Fracture of a C130 Aircraft Main Landing Gear Wheel Flange
Handbook of Case Histories in Failure Analysis
Failure of a Reversible Flap Valve in a Thermal Power Station
Handbook of Case Histories in Failure Analysis
Condition Assessment and Improvement of a Steam Turbine Rotor
Handbook of Case Histories in Failure Analysis
Fatigue Fracture of an Aluminum Alloy 7075-T73 Landing-Gear Torque Arm
ASM Failure Analysis Case Histories: Air and Spacecraft