Failure Analysis of Door Lock Assemblies Illustrating the Statistical Aspects of Failure Analysis
-
Published:2019
Abstract
Statistical techniques provide the design engineer with a powerful tool for the analysis of failure data. By means of an actual case study, steps required to design a test yielding statistically meaningful data and procedures used in graphical analysis of results are presented. The Weibull distribution is the statistical model used as a basis for these techniques. This method of failure analysis provides the engineer with clear, positive design direction.
J. Forgione, Failure Analysis of Door Lock Assemblies Illustrating the Statistical Aspects of Failure Analysis, ASM Failure Analysis Case Histories: Automobiles and Trucks, ASM International, 2019, https://doi.org/10.31399/asm.fach.auto.c9001732
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!