Abstract
Two examples concerning fabricated mild steel rotor spiders which failed due to lack of torsional rigidity, probably supplemented by the presence of high internal stress, are described. The machine concerned in the first case was a 3,000 hp three-phase slip-ring motor. In the second case the machine was a 200 kW alternator, direct-driven by a diesel engine running at 750 rpm. Both the foregoing failures reveal the same basic weakness, i.e., insufficient rigidity when subjected to variations or reversals of torque. In the first case, the bars welded to the arms were inadequately supported in a lateral direction, so...
Sign in
ASM members
Member Sign InFatigue Cracking of Welded Structures Under Dynamic Loading, ASM Failure Analysis Case Histories: Design Flaws, ASM International, 2019, https://doi.org/10.31399/asm.fach.design.c9001424
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!