Fracture of a 1040 Steel Fan Shaft Resulting From Use of an Improper Material
-
Published:2019
Abstract
The fan drive support shaft, specified to be made of cold-drawn 1040 to 1045 steel, fractured after 2240 miles of service. It was revealed by visual examination of the shaft that the fracture had initiated near the fillet at an abrupt change in shaft diameter. The cracks originated at two locations approximately 180 deg apart on the outer surface of the shaft and propagated toward the center. Features typical of reversed-bending fatigue were exhibited by the fracture. A tensile specimen was machined from the center of the shaft and it indicated much lower yield strength (369 MPa) than specified....
Sign in
ASM members
Member Sign InFracture of a 1040 Steel Fan Shaft Resulting From Use of an Improper Material, ASM Failure Analysis Case Histories: Design Flaws, ASM International, 2019, https://doi.org/10.31399/asm.fach.design.c0047850
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!