Retrieved Bone Screw Made From Co-Cr-Mo Alloy with Casting Defects
-
Published:2019
Abstract
Threads of a bone screw (Co-Cr-Mo alloy, type ASTM F75) had broken off, and other threads had cracked. 15x sectioning showed porosity, and 155x magnification showed gas holes, segregation, and dissolved oxides. This supports the conclusion that manufacturing defects caused the failure.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Retrieved Bone Screw Made From Co-Cr-Mo Alloy with Casting Defects, ASM Failure Analysis Case Histories: Medical and Biomedical Devices, ASM International, 2019, https://doi.org/10.31399/asm.fach.med.c0089543
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Broken Adjustable Moore Pins Made From Cobalt-Chromium Alloy
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Broken Stem of Femoral Head Component of Total Hip Prosthesis Made From Cast Cobalt-Base Alloy
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Metal Waves or Laking on Zinc-Based Diecastings
ASM Failure Analysis Case Histories: Processing Errors and Defects
Cracked Cast Iron Crankcases
ASM Failure Analysis Case Histories: Processing Errors and Defects
Failure of the Bond Between a Cobalt Alloy Prosthetic Casting and a Sintered Porous Coating
Handbook of Case Histories in Failure Analysis
Premature Torquing Failures of Cast A356 Aluminum Actuators
Handbook of Case Histories in Failure Analysis
Gray-Iron Paper-Drier Head Removed from Service
ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment
Cracking in a Gray-Iron Cylinder Head Caused by Microporosity
ASM Failure Analysis Case Histories: Automobiles and Trucks
Failure of Compound Bow Handle Risers
Handbook of Case Histories in Failure Analysis
Investigation on a Damaged Propeller Blade
ASM Failure Analysis Case Histories: Air and Spacecraft