Broken Adjustable Moore Pins Made From Cobalt-Chromium Alloy
-
Published:2019
Abstract
Two of four adjustable Moore pins, which had been used to stabilize a proximal femur fracture, were found to be broken and deformed at their threads. The pins were made from a cobalt-chromium alloy and were not in the same condition. Brittle precipitates in the grains and grain boundaries were seen in one of the pins and hence the fracture was revealed to have occurred along the grain boundaries. The other pin made from cold-worked cobalt-chromium alloy was observed to have randomly lines of primary inclusions. Intermingled dimples and fatigue striations were exhibited on the fracture surface of this...
Sign in
ASM members
Member Sign InBroken Adjustable Moore Pins Made From Cobalt-Chromium Alloy, ASM Failure Analysis Case Histories: Medical and Biomedical Devices, ASM International, 2019, https://doi.org/10.31399/asm.fach.med.c0048399
Download citation file:
2022 ASM International Catalog: Issue 1
View new, upcoming, and best-selling ASM Handbooks, technical books, and databases.