ASM Failure Analysis Case Histories: Household Products and Consumer Goods
Abstract
Failure analysis of a fishhook that broke during retrieval is described. Although the broken hook was discarded, several companion hooks were analyzed (chemistry, microhardness, metallographic cross section, and tensile properties) as were comparable products made by other hook manufacturers. Tensile test data indicated that the companion hooks were significantly different from hooks made by other manufacturers. The hooks broke into several pieces and failed with little or no plastic deformation, while hooks made by other manufacturers plastically deformed and did not break during testing.
Sign in
ASM members
Member Sign InJ.P. Sauer, Litagation Analysis Related to a Fragmented Fishhook, ASM Failure Analysis Case Histories: Household Products and Consumer Goods, ASM International, 2019, https://doi.org/10.31399/asm.fach.homegoods.c9001631
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.