The handle from a consumer product exhibited an apparent surface defect. The handle had been injection molded from a medium viscosity grade ABS resin. The anomalous appearance was objectionable to the assembler of the final product and resulted in a production lot being placed on quality-control hold. Investigation included visual inspection, 24x micrographs, and FTIR in the reflectance mode. The spectrum obtained on the included material was characteristic of polybutadiene, the rubber-modifying agent present in ABS. This supported the conclusion that the inclusion's most likely source was an undispersed gel particle formed during the production of the molding resin....