Brittle Fracture Leading to Failure of a Bridge Section
-
Published:2019
Abstract
A large crack developed at a girder-truss joint area of the Fremont bridge in Portland, OR, on 28 Oct 1971. It occurred during a positioning procedure involving a junction piece welded to a girder, starting as a brittle fracture and terminating in plastic hinges in the girder web welds. The arch rib top plate, as it met the main girder, formed a composite beam of A588/A36 composition. Investigation showed the original design of the failed component called for an angle of high geometric stress concentration (90 deg with no radius) in a region of substantial transverse weld joints. While...
Sign in
ASM members
Member Sign InHarry Czyzewski, Brittle Fracture Leading to Failure of a Bridge Section, ASM Failure Analysis Case Histories: Buildings, Bridges, and Infrastructure, ASM International, 2019, https://doi.org/10.31399/asm.fach.bldgs.c9001544
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.