ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment
Cracking in a Yankee Dryer Shell
-
Published:2019
Abstract
Cracking was found in the heads on large Yankee dryers, large, cylindrical, rotating, pressurized, high-temperature, cast iron pressure vessels (ASME Boiler and Pressure Vessel Code Section VIII, Rules for Construction of Pressure Vessels), used to remove moisture from sheets of tissue paper during manufacturing. The typical components consist of a cast iron shell, two cast iron concave heads, and a large cast iron internal center stay attached to journals. The heads are attached to the shell and center stay with high-strength bolts. FEA and metallurgical investigation supported the conclusion that the cracking was caused by an unexpected type of...
Sign in
ASM members
Member Sign InCracking in a Yankee Dryer Shell, ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.pulp.c0090276
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!