ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment
Shell and Head Cracking in Gray Cast Iron Paper Machine Dryer Rolls
-
Published:2019
Abstract
Several cases of failures in gray cast iron paper machine dryer rolls were evaluated. The rolls were found have ground outer cylindrical surfaces on which the paper web is dried. They were found to rotate about their longitudinal axes at speeds from 50 to 250 rpm while containing saturated steam from 35 to 380 kPa. Failures were found to occur in the shell body, in a head near a hand hole or a manhole opening, or in a head near the journal-to-head interface. A cleavage fracture was revealed by scanning electron microscopy regardless of the driving stress for failure....
Sign in
ASM members
Member Sign InShell and Head Cracking in Gray Cast Iron Paper Machine Dryer Rolls, ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.pulp.c0048804
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.