Grinding Plate Wear Failure Analysis
-
Published:2019
Abstract
A 230 mm (9 in.) diameter disk attrition mill was scheduled to grind 6.35 mm (0.25 in.) diameter quartz particles to a 0.075 mm (0.003 in.) diameter powder. Due to severe wear on the grinding plates, however, the unit was unable to complete the task of grinding the rock. The mill consisted of a heavy gray cast iron frame, a gravity feeder port, a runner, and a heavy-duty motor. The frame and gravity feeder weighed over 200 kg (440 lb) and, in some areas, was over 25 mm (1 in.) thick. To obtain the operating speed of 200 rpm,...
Sign in
ASM members
Member Sign InGrinding Plate Wear Failure Analysis, ASM Failure Analysis Case Histories: Machine Tools and Manufacturing Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.machtools.c0091853
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!