This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of two types of ceramics, namely, boron- and carbon-doped silicon carbide.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Ceramics: Atlas of Fractographs, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 471, https://doi.org/10.31399/asm.hb.v12.a0000627
Download citation file:
2022 ASM International Catalog: Issue 1
View new, upcoming, and best-selling ASM Handbooks, technical books, and databases.
Related Book Content
Ceramics
Machining
Friction and Wear of Ceramics
Friction, Lubrication, and Wear Technology
Concrete and Asphalt: Atlas of Fractographs
Fractography
Nickel Alloys: Atlas of Fractographs
Fractography
Resin-Matrix Composites: Atlas of Fractographs
Fractography
Cobalt Alloys: Atlas of Fractographs
Fractography
Metal-Matrix Composites: Atlas of Fractographs
Fractography
Martensitic Stainless Steels: Atlas of Fractographs
Fractography
Characterization of Ceramics and Glasses
Materials Characterization (2019 Edition)
Electronic Materials: Atlas of Fractographs
Fractography