Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of copper alloys and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the following: fatigue fracture, intergranular fracture, transgranular fracture, microvoid coalescence, corrosion fatigue, fatigue striations, tensile-overload fracture, stress-corrosion cracking, and pitting corrosion of these alloys.