Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of nickel alloys and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the fatigue crack, transgranular cleavage, intergranular fracture, grain boundaries, notch and fatigue precrack, dimpled rupture, and fatigue striations of these alloys.
You do not currently have access to this chapter.
Citation
Nickel Alloys: Atlas of Fractographs, Fractography, Vol 12, By ASM Handbook Committee, ASM International, 1987, p 396–401, https://doi.org/10.31399/asm.hb.v12.a0000617
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Cemented Carbides: Atlas of Fractographs
Fractography
ASTM/ASME Alloy Steels: Atlas of Fractographs
Fractography
Pure Irons: Atlas of Fractographs
Fractography
Low-Carbon Steels: Atlas of Fractographs
Fractography
Austenitic Stainless Steels: Atlas of Fractographs
Fractography
Concrete and Asphalt: Atlas of Fractographs
Fractography
Ceramics: Atlas of Fractographs
Fractography
AISI/SAE Alloy Steels: Atlas of Fractographs
Fractography