Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of gray irons and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the fatigue fracture, solidification structure, and crack propagation of gray irons.
You do not currently have access to this chapter.
Citation
Gray Irons: Atlas of Fractographs, Fractography, Vol 12, By ASM Handbook Committee, ASM International, 1987, p 225–226, https://doi.org/10.31399/asm.hb.v12.a0000602
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Cobalt Alloys: Atlas of Fractographs
Fractography
Martensitic Stainless Steels: Atlas of Fractographs
Fractography
Maraging Steels: Atlas of Fractographs
Fractography
High-Carbon Steels: Atlas of Fractographs
Fractography
Tool Steels: Atlas of Fractographs
Fractography
Copper Alloys: Atlas of Fractographs
Fractography
Microstructural Features of Prematurely Failed Hot-Strip Mill Work Rolls: Some Studies in Spalling Propensity
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
Low-Carbon Steels: Atlas of Fractographs
Fractography
Medium-Carbon Steels: Atlas of Fractographs
Fractography