Abstract
This article is an atlas of fractographs that covers nickel-base superalloys. The fractographs display the following: hydrogen-embrittlement fracture; segment of a fractured second-stage gas-turbine wheel; gas-producer turbine rotor cast; dendritic stress-rupture fracture surface; fatigue and creep fractures; simultaneous metallographic-fractographic evaluation; and effect of thermal cycling on fatigue fracture.
You do not currently have access to this chapter.
Citation
Nickel-Base Alloys: Atlas of Fractographs, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 389–395, https://doi.org/10.31399/asm.hb.v12.a0000616
Download citation file:
Related Book Content
Fracture Appearance and Mechanisms of Deformation and Fracture
Failure Analysis and Prevention (2021 Edition)
Fracture Appearance and Mechanisms of Deformation and Fracture
Failure Analysis and Prevention
Additive Manufacturing of Nickel-Base Superalloys
Additive Manufacturing Processes
Macroetchants for Revealing Strain Patterns in Nonferrous Metals
Metallography Principles and Practice
Creep
Damage Mechanisms and Life Assessment of High-Temperature Components
Nonequilibrium Reactions Precipitation Hardening
Phase Diagrams Understanding the Basics
Modeling of Microstructure Evolution during the Thermomechanical Processing of Nickel-Base Superalloys
Fundamentals of Modeling for Metals Processing
Polycrystalline Cast Superalloys
Properties and Selection: Irons, Steels, and High-Performance Alloys
Pump Shaft Failure
ASM Failure Analysis Case Histories: Design Flaws
Failure of a Throttle End Fitting in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories