Pure Irons: Atlas of Fractographs
-
Published:1987
Abstract
This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of pure irons and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the grain-boundary cavitation; slip lines; intergranular fracture; cleavage fracture; notch-impact fracture; oxide inclusions and blowholes; ductile rupture; impact fracture and tensile-test fracture surfaces; fatigue striations; and crack initiation and propagation of pure irons.
You do not currently have access to this chapter.
Citation
Pure Irons: Atlas of Fractographs, Fractography, Vol 12, ASM Handbook, By ASM Handbook Committee, ASM International, 1987, p 219–224, https://doi.org/10.31399/asm.hb.v12.a0000601
Download citation file:
Related Book Content
AISI/SAE Alloy Steels: Atlas of Fractographs
Fractography
Titanium Alloys: Atlas of Fractographs
Fractography
Low-Carbon Steels: Atlas of Fractographs
Fractography
Nickel Alloys: Atlas of Fractographs
Fractography
Cemented Carbides: Atlas of Fractographs
Fractography
ASTM/ASME Alloy Steels: Atlas of Fractographs
Fractography
Tool Steels: Atlas of Fractographs
Fractography
Fracture Analysis
Cast Iron Science and Technology
High-Carbon Steels: Atlas of Fractographs
Fractography