Brazing of Ceramic and Ceramic-to-Metal Joints
-
Published:1993
Abstract
This article is intended to assist the development of procedures for the brazing of ceramic-to-ceramic or ceramic-to-metal joints for service under elevated temperatures, mechanical or thermal stresses, or corrosive atmospheres. It describes the factors considered in preparing a procedure for the brazing of graphitic materials.
Sign in
ASM members
Member Sign InA.J. Moorhead, W.H. Elliott, Jr., H.-E. Kim, Brazing of Ceramic and Ceramic-to-Metal Joints, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 948–960, https://doi.org/10.31399/asm.hb.v06.a0001457