Overview of Weld Discontinuities
-
Published:1993
Abstract
This article provides an overview of the types of weld discontinuities that are characteristic of specialized welding processes. These welding processes include electron-beam welding, plasma arc welding, electroslag welding, friction welding, resistance welding, and diffusion welding. The article also describes the common inspection methods used to detect these discontinuities.
You do not currently have access to this chapter.
Citation
Overview of Weld Discontinuities, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1073–1080, https://doi.org/10.31399/asm.hb.v06.a0001472
Download citation file:
Related Book Content
Welding of Zirconium Alloys
Welding, Brazing, and Soldering
Welding of Titanium Alloys
Welding, Brazing, and Soldering
Selection of Wrought Martensitic Stainless Steels
Welding, Brazing, and Soldering
Weld Discontinuities and Imperfections
Weld Integrity and Performance
Selection and Weldability of Aluminum Metal-Matrix Composites
Welding, Brazing, and Soldering
Joining of Oxide-Dispersion-Strengthened Materials
Welding, Brazing, and Soldering
Solid-State Welding and Bonding
Joining Understanding the Basics
Welding in Space and Low-Gravity Environments
Welding, Brazing, and Soldering
Safe Practices
Welding, Brazing, and Soldering
Arc Welding of Metals
Joining Understanding the Basics