Weldments exhibit special microstructural features that need to be recognized and understood in order to predict acceptable corrosion service life of welded structures. This article describes some of the general characteristics associated with the corrosion of weldments. It emphasizes the role of macrocompositional and microcompositional variations to bring out differences that need to be realized in comparing corrosion of weldments to that of wrought materials. The article concludes with a discussion on important welding practices used to minimize corrosion in weldments.
A. Wahid, D.L. Olson, D.K. Matlock, C.E. Cross, Corrosion of Weldments, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1065–1069, https://doi.org/10.31399/asm.hb.v06.a0001471
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!