Welding, Brazing, and Soldering
Joining of Oxide-Dispersion-Strengthened Materials
-
Published:1993
Abstract
Oxide - dispersion - strengthened (ODS) materials utilize extremely fine oxide dispersion for strengthening, such as nickel-base alloys or alumina. The processing techniques employed in the production of ODS alloys produce some entrapped gases, which tend to create porosity during welding that can be rectified by suitable designing considerations. This article discusses certain successful design strategies employed in joining ODS alloys in consideration with the grain structure. It further provides a brief discussion on different welding processes involved in joining ODS materials, namely, gas-tungsten arc welding, gas-metal arc welding, electron-beam and laser-beam welding, resistance welding, furnace brazing, friction welding,...
Sign in
ASM members
Member Sign InDavid O'Donnell, Joining of Oxide-Dispersion-Strengthened Materials, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1037–1040, https://doi.org/10.31399/asm.hb.v06.a0001467
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!