Characterization and Modeling of the Heat Source
-
Published:1993
Abstract
This article briefly reviews the physical phenomena that influence the input-energy distribution. It discusses the several simplified and detailed heat source models used in the modeling of arc welding, high-energy-density welding, and resistance welding processes.
S.S. Glickstein, E. Friedman, Characterization and Modeling of the Heat Source, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 1141–1146, https://doi.org/10.31399/asm.hb.v06.a0001481