Selection of Nickel-Base Corrosion-Resistant Alloys Containing Molybdenum
By
S.J. Matthews
S.J. Matthews
Haynes International, Inc.
Search for other works by this author on:
-
Published:1993
Abstract
This article discusses the welding characteristics, welding metallurgy, and postweld heat treatment process of nickel-base corrosion-resistant alloys containing molybdenum. It contains tables that provide information on the nominal chemical compositions and physical properties of the alloys.
You do not currently have access to this chapter.
Citation
S.J. Matthews, Selection of Nickel-Base Corrosion-Resistant Alloys Containing Molybdenum, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 593–597, https://doi.org/10.31399/asm.hb.v06.a0001429
Download citation file:
Related Book Content
Metallurgical Failure Analysis of Cold Cracking in a Structural Steel Weldment: Revisiting a Classic Failure Mechanism
ASM Failure Analysis Case Histories: Buildings, Bridges, and Infrastructure
The Materials Selection Process
Metallurgy for the Non-Metallurgist (Second Edition)
Postweld Heat Treatment of Nonferrous High-Temperature Materials
Welding, Brazing, and Soldering
Properties of Metals
Metals Handbook Desk Edition (2nd Edition)
Hot-Work Tool Steels
Tool Steels (Fifth Edition)
Modeling of Diffusion Bonding
Metals Process Simulation
Alloy 430 Ferritic Stainless Steel Welds Fail due to Stress-Corrosion Cracking in Heat-Recovery Steam Generator
ASM Failure Analysis Case Histories: Power Generating Equipment
Materials for Advanced Steam Plants
Damage Mechanisms and Life Assessment of High-Temperature Components
Erosion and Erosion-Corrosion
High-Temperature Corrosion and Materials Applications
Introduction to the Effects of Composition, Processing, and Structure on Materials Properties
Materials Selection and Design