Book Chapter
Quality Assurance of Metal-Matrix Composites
By
William C. Harrigan, Jr.
William C. Harrigan, Jr.
MMC Engineering, Inc.
Search for other works by this author on:
-
Published:2001
Publication history
November 01, 2001
Abstract
This article describes the characterization techniques, mechanical tests, and nondestructive evaluation methods that are commonly used for metal-matrix composites. It also tabulates typical methods of particle size and size distribution measurement, as well as mechanical test specifications for aluminum-matrix composites.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
William C. Harrigan, Jr., Quality Assurance of Metal-Matrix Composites, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 726–730, https://doi.org/10.31399/asm.hb.v21.a0003437
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Metal-Matrix Composites
Elements of Metallurgy and Engineering Alloys
Metal-Matrix Composites
Metals Handbook Desk Edition (2nd Edition)
Metal-Matrix Composites
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Age Forming
Metalworking: Sheet Forming
Quality Control and Quality Assurance
Steel Castings Handbook (Sixth Edition)
Corrosion of Aluminum Metal-Matrix Composites
Corrosion of Aluminum and Aluminum Alloys
Sampling
Materials Characterization
Modeling and Simulation of the Heat Treatment of Aluminum Alloys
Heat Treating of Nonferrous Alloys
Particle-Induced X-Ray Emission
Materials Characterization