Abstract
This article provides a summary of the concepts discussed in the articles under the Section “Failure Analysis” in ASM Handbook, Volume 21: Composites. Most of the information in this Section is geared toward organic-matrix composites, although there is some information on failure analysis and fractography of ceramic- and metal-matrix composites.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Patricia L. Stumpff, Introduction to Failure Analysis, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 949–950, https://doi.org/10.31399/asm.hb.v21.a0003460
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Introduction to Composites
Composites
Introduction to Post-Processing and Assembly
Composites
Introduction to Reinforcing Fibers
Composites
Rapid Prototyping
Composites
Design with Composites
Materials Selection and Design
The Failure Analysis Process
Fatigue and Fracture Understanding the Basics
Joining of Organic-Matrix Composites
Welding, Brazing, and Soldering
Tensile Testing of Ceramics and Ceramic-Matrix Composites
Tensile Testing (Second Edition)