Composites
Tooling and Assembly Quality Control
-
Published:2001
Abstract
Tooling and assembly methodologies for advanced composites have steadily improved as a result of advancements in materials, through the use of computer-aided design/computer-aided manufacturing technology, and through application of sophisticated design for manufacturing and assembly concepts. This article reviews techniques and technologies that are used to control the quality of tooling and assembly methods for composite components.
Sign in
ASM members
Member Sign InTooling and Assembly Quality Control, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 682–684, https://doi.org/10.31399/asm.hb.v21.a0003433
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.