Design for Fatigue Resistance
-
Published:1997
Abstract
The design of components against fatigue failure may involve several considerations of irregular loading, variable temperature, and environment. This article focuses on design considerations against fatigue related to material performance under mechanical loading at constant temperature. It reviews the traditional methods of fatigue design on smooth and notched components. The article discusses high-cycle fatigue in terms of fatigue strength and tensile strength, mean stress effects, stress concentration, and multiaxial fatigue. It describes low-cycle fatigue in terms of deformation behavior and concludes with a discussion on lifetime analysis based on a strain approach.
Sign in
ASM members
Member Sign InErhard Krempl, Design for Fatigue Resistance, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 516–532, https://doi.org/10.31399/asm.hb.v20.a0002469
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.