Materials Selection and Design
Design for Plastics Processing
-
Published:1997
Abstract
This article describes key processing methods and related design, manufacturing, and application considerations for plastic parts. The methods include injection molding, extrusion, thermoforming, blow molding, rotational molding, compression molding/transfer molding, composites processing, and casting. The article describes principal features incorporated into the design of plastic parts. It concludes with a discussion on the materials selection methodology for plastics.