Materials Selection and Design
Design for Wear Resistance
-
Published:1997
Abstract
Wear is the damage to a solid surface as a result of relative motion between it and another surface or substance. This article discusses the four general ways by which a material can wear, namely, adhesive wear, abrasive wear, fatigue or fatigue-like wear, and corrosive wear. It tabulates the operational classification of wear situations and describes the relationship between wear or wear rate and design parameters. The article reviews the effect of lubrication on wear behavior and the types of lubricants. It illustrates some fundamental criteria that can be applied in the selection of a material for wear applications. The article explains four elements of wear design, such as system analysis, modeling, data gathering, and verification. It concludes with a discussion on the design approach for low-wear computer peripherals.
Raymond G. Bayer, Design for Wear Resistance, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 603–614, https://doi.org/10.31399/asm.hb.v20.a0002474
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!