Book Chapter
Performance Indices
By
M.F. Ashby
M.F. Ashby
Engineering Design Centre, Cambridge University
Search for other works by this author on:
-
Published:1997
Abstract
This article defines performance indices in a formal way and specifies how they are derived. The performance indices for a light, strong tie and a light, stiff beam are presented. The article presents two case studies that illustrate the use of material indices, shape factors, and selection charts to select materials.
Topics
Properties and performance
You do not currently have access to this chapter.
Citation
M.F. Ashby, Performance Indices, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 281–290, https://doi.org/10.31399/asm.hb.v20.a0002453
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Design Guidelines for Advanced High-Strength Steels
Advanced-High Strength Steels Science, Technology, and Applications
The Materials Selection Process
Metallurgy for the Non-Metallurgist (Second Edition)
Modeling of Diffusion Bonding
Metals Process Simulation
Selection and Weldability of Non-Heat-Treatable Aluminum Alloys
Welding, Brazing, and Soldering
Introduction to the Effects of Composition, Processing, and Structure on Materials Properties
Materials Selection and Design
Erosion and Erosion-Corrosion
High-Temperature Corrosion and Materials Applications
Materials for Advanced Steam Plants
Damage Mechanisms and Life Assessment of High-Temperature Components
Material Property Charts
Materials Selection and Design
Porous Powder Metallurgy Technology
Powder Metallurgy
Introduction and Overview of Design Considerations and Materials Selection
Metals Handbook Desk Edition (2nd Edition)