Abstract
This article focuses on the industrial applications of phase diagrams. It presents examples to illustrate how a multicomponent phase diagram calculation can be readily useful for industrial applications. The article demonstrates how the integration of a phase diagram calculation with kinetic and microstructural evolution models greatly enhances the power of the CALPHAD approach in materials design and processing development. It also discusses the limitations of the CALPHAD approach.
Sign in
ASM members
Member Sign InF. Zhang, Y. Yang, W.S. Cao, S.L. Chen, K.S. Wu, Y.A. Chang, Commercial Alloy Phase Diagrams and Their Industrial Applications, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010, p 117–131, https://doi.org/10.31399/asm.hb.v22b.a0005511
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!