Abstract
This article presents a table that lists the linear thermal expansion of selected metals and alloys. These include aluminum, copper, iron, lead, magnesium, nickel, tin, titanium, and zinc and their alloys. Thermal expansion is presented for specific temperature ranges.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Linear Thermal Expansion of Metals and Alloys, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 602–603, https://doi.org/10.31399/asm.hb.v22a.a0005443
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Thermal Conductivity of Metals and Alloys
Fundamentals of Modeling for Metals Processing
Density of Metals and Alloys
Fundamentals of Modeling for Metals Processing
Heat Treating of Nonferrous Alloys
Metals Handbook Desk Edition (2nd Edition)
Heat Treatable Nonferrous Alloys
Heat Treating of Nonferrous Alloys
Metallography and Microstructures of Zinc and Its Alloys
Metallography and Microstructures
Density of Metals and Alloys
Corrosion: Materials
Heat Treatment of Nonferrous Alloys
Metallurgy for the Non-Metallurgist (Second Edition)
Heat Treatment of Aluminum and Other Nonferrous Alloys
Practical Heat Treating Basic Principles
Foundry Practice for Nonferrous Alloys
Metals Handbook Desk Edition (2nd Edition)
Effects of Composition, Processing, and Structure on Properties of Nonferrous Alloys
Materials Selection and Design