Lubrication and Wear in Forging
-
Published:2017
Abstract
Both hot and cold forgings are batch-type processes in which steady-state conditions are never fully achieved and the initial lubricant supply must perform adequately for the duration of the operation. This article discusses methods to measure lubricant effectiveness and wear. It describes the mixed-film lubrication and solid film lubrication in cold forging, as well as solid film lubrication and thick film lubrication in hot forging. The article reviews the factors affecting abrasive wear: die hardness, workpiece temperature, and lubrication and die temperature. It concludes with information on ways to improve resistance to abrasive wear.
Sign in
ASM members
Member Sign InK.D. Clarke, C.J. Van Tyne, Lubrication and Wear in Forging, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 798–807, https://doi.org/10.31399/asm.hb.v18.a0006424
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.