Friction, Lubrication, and Wear Technology
Wear Measurement
Revising author
Revising author
Revising author
-
Published:2017
Abstract
This article describes the determination of wear loss by measuring either mass change or dimensional change of lubricants and materials. It discusses the principles, advantages and disadvantages of mass loss measures and dimensional measures of wear. The article details wear measurement at the nanoscale, such as atomic force microscopy (AFM) measurement and scanning electron microscopy measurement. It reviews the techniques of wear measurement at the atomic level, namely, transmission electron microscopy (TEM) measurement and AFM combined with TEM measurement.
Linmao Qian, Lei Chen, Liang Jiang, Wear Measurement, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 225–232, https://doi.org/10.31399/asm.hb.v18.a0006387
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.