Friction, Lubrication, and Wear Technology
Fundamentals of Lubrication
-
Published:2017
Abstract
This article provides a brief introduction to lubrication as a method to reduce friction between two surfaces. It discusses the surface characteristics of parts and explores how lubrication helps separate two contacting surfaces and thereby decreases the coefficient of friction. The article details the classifications of lubrication regimes, namely, boundary, mixed, hydrodynamic, and elastohydrodynamic lubrications. It discusses the various types of lubricant materials and additives, including liquid lubricants, solid lubricants, gaseous lubricants, greases, green lubricants, and nanomaterials. The article also reviews the properties of lubricants. It describes the tribological evaluation of lubricants, including stribeck test, four-ball test, block-on-ring test, pin-in-vee test, and reciprocating motion test.
Suresh C. Kuiry, Fundamentals of Lubrication, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 105–117, https://doi.org/10.31399/asm.hb.v18.a0006401
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!