Lubrication Strategies for Extreme Environments
By
Gary Doll
Gary Doll
The University of Akron
Search for other works by this author on:
-
Published:2017
Abstract
Strategies for the lubrication of mechanical systems operating in extreme environments must exclude the liquid lubricants and greases and rely on alternative methods of lubrication, such as gases and solids. This article provides a survey of some of the more effective alternative methods of lubrication. It provides a discussion on the solid materials that have been most commonly used as lubricants: carbon-base materials, transition metal dichalcogenides, polymers, and soft metals.
You do not currently have access to this chapter.
Citation
Gary Doll, Lubrication Strategies for Extreme Environments, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 213–219, https://doi.org/10.31399/asm.hb.v18.a0006369
Download citation file:
Related Book Content
Fundamentals of Lubrication
Friction, Lubrication, and Wear Technology
Friction and Wear Testing
Characterization and Failure Analysis of Plastics
Transition Metal Dichalcogenide-Based (MoS 2 , WS 2 ) Coatings
Friction, Lubrication, and Wear Technology
Friction and Wear Testing
Characterization and Failure Analysis of Plastics
Friction and Wear Testing of Polymers
Engineered Materials Handbook Desk Edition
Tribology of Lubricants
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Lubrication and Wear in Drawing Operations
Friction, Lubrication, and Wear Technology
Lubricants for Rolling-Element Bearings
Friction, Lubrication, and Wear Technology
Solid Lubricants
Friction, Lubrication, and Wear Technology
Temperature, Strain, and Magnetic Field Measurements
Materials at Low Temperatures