This article reviews specific processing characteristics and forging-related properties of commonly forged families of metals and alloys, including carbon and alloy steels, stainless steels, heat-resistant alloys (iron, cobalt, and nickel base alloys), aluminum alloys, copper and copper alloys, magnesium alloys, and titanium alloys. It provides forging process variables such as stock preparation, heating and cooling of forgings, die lubrication, trimming, and cleaning of these metals and alloys. The article explains the effect of temperature, deformation rate, and die temperature on forgeability and describes the forging methods of these metals and alloys.
Forging of Specific Metals and Alloys, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 863–875, https://doi.org/10.31399/asm.hb.mhde2.a0003184
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.