Zirconium and Hafnium
-
Published:1998
Abstract
This article discusses the general characteristics, primary and secondary fabrication methods, product forms, and corrosion resistance of zirconium and hafnium. It describes the physical metallurgy of zirconium and its alloys, providing details on allotropic transformation and anisotropy that profoundly influences the engineering properties of zirconium and its alloys. Tables listing the values for chemical composition and tensile properties for nuclear and nonnuclear grades of zirconium are also provided.
Topics
Properties and performance,
Material failure analysis,
Fractography,
Cast iron,
Steel,
Stainless steel,
High-strength low-alloy steel,
Steel powder,
Superalloys,
Metallography,
Metal-matrix composites,
Aluminum,
Processing, treatment, and fabrication,
Corrosion,
Zirconium alloys,
Chemical composition,
Tensile properties,
Hafnium,
Zirconium
You do not currently have access to this chapter.
Citation
Zirconium and Hafnium, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 621–623, https://doi.org/10.31399/asm.hb.mhde2.a0003149
Download citation file:
Related Book Content
Zirconium and Hafnium
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Stress-Corrosion Cracking of Zirconium Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Corrosion in the Food and Beverage Industries
Corrosion: Environments and Industries
Miscellaneous Nonferrous Metals
Elements of Metallurgy and Engineering Alloys
Nickel and Nickel Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Metallography and Microstructures of Zirconium, Hafnium, and Their Alloys
Metallography and Microstructures
Selection of Wrought Duplex Stainless Steels
Welding, Brazing, and Soldering
Corrosion by Ammonia
Corrosion: Environments and Industries
Corrosion of Nonferrous Alloy Weldments
Corrosion of Weldments
Welding of Zirconium Alloys
Welding, Brazing, and Soldering