Wear-Resistant Austenitic Manganese Steels
-
Published:1998
Abstract
Hadfield's austenitic manganese steel exhibits high toughness and ductility with high work-hardening capacity and, usually, good wear resistance. Beginning with an overview of the as-cast properties and composition of these class of steels, this article discusses the heat treatment methods used to improve their wear resistance, and the changes in the mechanical properties after heat treatment. Manganese steels are unequaled in their ability to work harden, exceeding even the metastable austenitic stainless steels in this feature.
Sign in
ASM members
Member Sign InWear-Resistant Austenitic Manganese Steels, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 266–269, https://doi.org/10.31399/asm.hb.mhde2.a0003102
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!