Precious Metals and Alloys
-
Published:1998
Abstract
Precious metals include gold, silver, and six platinum-group metals, namely, platinum, palladium, ruthenium, rhodium, osmium, and iridium. This article focuses on the consumption, trade practices, properties, product forms, and applications of these metals and their alloys.
You do not currently have access to this chapter.
Citation
Precious Metals and Alloys, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 624–628, https://doi.org/10.31399/asm.hb.mhde2.a0003150
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Corrosion of Precious Metals and Alloys
Corrosion: Materials
Miscellaneous Nonferrous Metals
Elements of Metallurgy and Engineering Alloys
Noble and Precious Metal Applications in Biomaterials with Emphasis on Dentistry
Materials for Medical Devices
Properties of Precious Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Heat-Treatable Aluminum Alloy Temper Designations
Aluminum: Technology, Industry, and Applications
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Annealing of Precious Metals
Heat Treating of Nonferrous Alloys
History of Powder Metallurgy
Powder Metallurgy
Precious Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Stress-corrosion Fracture in Silver Solid-State Bonds of Uranium
Handbook of Case Histories in Failure Analysis