Engineered Materials Handbook Desk Edition
Abstract
A thermosetting resin, or thermoset, is a synthetic organic polymer that cures to a solid, infusible mass by forming a three-dimensional network of covalent chemical bonds. Significant applications include construction and thermoset engineering plastics. This article discusses the general and family characteristics of thermosetting resin families, including allyls, aminos (urea formaldehyde and melamine formaldehyde), cyanates, epoxies, polybenzimidazoles, unsaturated polyesters, thermoset polyimides, phenolics, and vinyl esters. It also explains processing methods, including curing and curing agents. The article provides descriptions of commercial product forms and the wide array of applications of thermosetting resins. It also tabulates the performance properties (mechanical,...
Sign in
ASM members
Member Sign InThermosets, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 250–281, https://doi.org/10.31399/asm.hb.emde.a0003010
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.