Abstract
Bulk molding compounds can be molded into a variety of complex shapes by methods that can be readily automated for high volume production. This article describes the formulation and processing (compound formation, and molding methods) of bulk molding compounds. It discusses the effects of fiber type, fiber length, and matrix type on thermoset bulk molding compounds. The markets for long-fiber-reinforced bulk molding compounds are electrical, ordnance, aerospace, industrial, sporting goods, and automotive applications.
Topics
Characterization, testing, and analysis,
Properties and performance,
Adhesives,
Ceramics,
Glasses,
Polymers,
Plastics,
Ceramic-matrix composites,
Polymer-matrix composites,
Processing, treatment, and fabrication,
Material applications and product forms,
Thermosetting matrices,
Fibers,
Bulk molding compounds
You do not currently have access to this chapter.
Citation
Bulk Molding Compounds, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 532–534, https://doi.org/10.31399/asm.hb.emde.a0003034
Download citation file:
Related Book Content
Composites
Elementary Materials Science
Industrial Applications of Steel Castings
Steel Castings Handbook (Sixth Edition)
Discontinuous-Fiber Composites
Structural Composite Materials
Heat Treatment of Gears
Heat Treatment of Gears A Practical Guide for Engineers
Explosion Welding
Welding, Brazing, and Soldering
Commercial Alloy Phase Diagrams and Their Industrial Applications
Metals Process Simulation
Precious Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Engineering Thermoplastics
Engineered Materials Handbook Desk Edition
Corrosion of Nickel and Nickel-Base Alloys
Corrosion: Materials
Molding Compounds
Composites