Rotational molding is a simple but unique process that has the capability of producing small to large hollow items with very uniform wall thicknesses. Providing an overview of the operating principles of rotational molding, this article discusses the key selection factors, including function and property requirements for resins and additives; size, shape, design, and cost of molded parts; equipment type and size; and the type of mold to be used. Commonly used molds include cast aluminum, fabricated sheet metal, nickel deposit, machined aluminum, silicone, fiberglass, and prototype molds.
Rotational Molding, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 321–326, https://doi.org/10.31399/asm.hb.emde.a0003017
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.