Analysis of Creep and Creep-Rupture Data[1],[2]
By
M.K. Booker
M.K. Booker
Oak Ridge National Laboratory
Search for other works by this author on:
-
Published:2000
Abstract
This article presents typical problems encountered in the analysis of experimental creep and creep-rupture data and the possible solutions to these drawbacks. It provides information on planning the test and creep strain/time relationships. The exponential creep equation and the rational polynomial creep equation are discussed. The article also describes the dependence of stress and temperature on equation parameters and explains the lot-centered regression analysis.
You do not currently have access to this chapter.
Citation
M.K. Booker, Analysis of Creep and Creep-Rupture Data,, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, https://doi.org/10.31399/asm.hb.v08.a0009218
Download citation file:
Related Book Content
Elevated-Temperature Failures
Understanding How Components Fail (Third Edition)
Modeling Creep Fatigue
Fundamentals of Modeling for Metals Processing
Creep, Stress Relaxation, and Yielding
Characterization and Failure Analysis of Plastics
Design for High-Temperature Applications
Materials Selection and Design
Creep and Stress-Rupture Failures
Failure Analysis and Prevention (2021 Edition)
Failure Analysis of Gas Turbine Last Stage Bucket Made of Udimet 500 Superalloy
ASM Failure Analysis Case Histories: Power Generating Equipment
Creep
Elements of Metallurgy and Engineering Alloys
Superplastic Deformation at Elevated Temperatures
Mechanical Testing and Evaluation
Fatigue and Fracture of Nickel-Base Superalloys
Fatigue and Fracture
Mechanical Behavior
Elementary Materials Science