Mechanical Testing and Evaluation
Gage Repeatability and Reproducibility in Hardness Testing[1]
-
Published:2000
Abstract
The gage repeatability and reproducibility (GRR) study is a procedure for determining the repeatability of a test instrument and the reproducibility of a specific gage in operation. This article reviews the general method of GRR studies and its application for indentation hardness testing. It describes a long method and a short method for evaluation of GRR. The article analyzes factors of hardness testing instruments and provides guidelines for hardness tests. It concludes with a list of suggestions that can improve hardness tests.
Edward L. Tobolski, Gage Repeatability and Reproducibility in Hardness Testing, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 278–281, https://doi.org/10.31399/asm.hb.v08.a0003277
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.