Sliding Contact Damage Testing
-
Published:2000
Abstract
Surface damage from sliding contact is related to the adhesion of mating surfaces in contact. This article describes the methods for evaluation of surface damage caused by sliding contact. It defines adhesive wear in terms of asperity, cold welding, galling, scuffing, seizure, and wear coefficient. The article discusses various galling testing methods, such as button-on-block galling test, pin-on-flat galling test, and threaded connection galling test. It provides an overview of fretting wear that occurs between two tight-fitting surfaces subjected to a cyclic, relative motion of extremely small amplitude. The article also reviews the fretting rig for investigating fretting wear.
Sliding Contact Damage Testing, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 346–358, https://doi.org/10.31399/asm.hb.v08.a0003285
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.