Mechanical Testing and Evaluation
Indentation Hardness Testing of Ceramics
-
Published:2000
Abstract
Hardness characterizes the resistance of the ceramic to deformation, densification, displacement, and fracture. It is usually measured with conventional microindentation hardness machines using the Knoop or the Vickers diamond indenters. This article discusses the metrology issues of the Knoop and the Vickers hardness in ceramics. It explicates how to estimate fracture toughness from Vickers indentation cracking. The article also provides information on instrumented hardness testing and the Meyer law.
Sign in
ASM members
Member Sign InG.D. Quinn, Indentation Hardness Testing of Ceramics, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 244–251, https://doi.org/10.31399/asm.hb.v08.a0003274
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.