Abstract
This article describes the principal methods for macroindentation hardness testing by the Brinell, Vickers, and Rockwell methods. For each method, the test types and indenters, scale limitations, testing machines, calibration, indenter selection and geometry, load selection and impression size, testing methodology, and testing of specific materials are also discussed.
Edward L. Tobolski, Andrew Fee, Macroindentation Hardness Testing, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 203–220, https://doi.org/10.31399/asm.hb.v08.a0003271